What Causes Uneven Resin Distribution in RTM Molding?

Nov 18, 2026 Weitong Fiberglass

RTM is a closed-mold process used to manufacture fiber-reinforced composite parts. During production, dry fiber reinforcement is placed inside a mold. Liquid resin is then injected into the cavity under pressure to impregnate the fiber preform.

If resin flow is restricted or filling rates vary significantly across the mold, defects such as dry spots, voids, incomplete impregnation, and resin-rich areas may occur. These problems are commonly associated with reinforcement permeability, resin properties, injection parameters, and mold design.

Main Causes of Uneven Resin Distribution in RTM Molding

1. Inconsistent Permeability of Fiber Reinforcement

The structure of the reinforcement directly affects resin flow. Under otherwise similar conditions, a higher fiber volume fraction and narrower pore channels generally reduce preform permeability, increasing resistance to resin flow.

If fiber arrangement, layup orientation, or compaction varies across the preform, resin may preferentially flow through areas with lower resistance, leaving other regions inadequately impregnated. When multiple reinforcement materials are combined, differences in permeability between layers must also be considered.

▸ Closed Mold Mat CF consists of a synthetic nonwoven core with chopped glass fibers laminated on both sides. It can be used in RTM and other closed-mold processes. Selecting a suitable material structure and layup can help improve resin flow and thickness consistency, although the actual results depend on the molding conditions.

2. Excessive Resin Viscosity or Unsuitable Gel Time

Resin viscosity affects how easily resin flows through the gaps between fibers. Excessively high viscosity increases flow resistance and may extend mold filling time. If the resin begins to gel before filling is complete, its flowability gradually decreases, making it difficult to impregnate unfilled areas.

Resin temperature, mixing ratio, and working time should therefore be controlled according to the resin system to maintain suitable flow characteristics during injection.

3. Improper Injection Pressure and Flow Rate

Injection pressure and flow rate must be matched to reinforcement permeability and resin viscosity. Insufficient pressure may slow mold filling and increase the risk of premature gelation. Excessive pressure or flow rate, however, may cause the fiber preform to shift, deform, or become locally compacted, changing the intended resin flow paths.

Simply increasing injection pressure is not a reliable solution to poor impregnation. Process settings should be determined according to mold dimensions, reinforcement structure, and the resin's processing window.

4. Poor Gate, Vent, or Mold Gap Design

The position and number of injection gates influence resin flow direction. Poor gate placement may cause some areas to fill before others are adequately impregnated.

Vent design is equally important. When resin flow fronts from different directions meet, trapped air may remain inside the reinforcement if it cannot escape through the vents. This can lead to voids or localized dry spots.

In addition, excessive gaps between the reinforcement and mold surface may allow resin to flow rapidly along low-resistance paths, bypassing parts of the fiber preform. This phenomenon is known as race tracking and can result in incomplete internal impregnation.

Common Resin Distribution Defects and Troubleshooting

Defect Possible Causes What to Check
Localized dry spots or unimpregnated fibers Uneven permeability, high viscosity, or insufficient filling time Layup structure, resin condition, and filling time
Internal voids Inadequate venting or trapped air where flow fronts meet Vent locations and flow-front convergence areas
Uneven edge impregnation Race tracking or excessive mold gaps Preform fit along the edges and mold sealing
Inconsistent thickness or fiber distribution Improper positioning, uneven compaction, or excessive injection pressure Layup thickness, preform fixation, and injection settings

⚑ Dry spots and voids should be distinguished during troubleshooting. A dry spot is an area where the reinforcement has not been adequately impregnated with resin, while a void is an air or gas-filled space trapped inside the finished part. Both defects may occur together, but they require different inspection approaches.

How to Improve Resin Distribution in RTM Molding

  • Check the reinforcement layup: Maintain consistent layup thickness and compaction, avoid localized material buildup, and evaluate the permeability of combined reinforcement layers.
  • Control resin conditions: Adjust resin temperature and mixing ratio according to the resin system, ensuring injection is completed within the applicable working time.
  • Optimize injection parameters: Set appropriate injection pressure, flow rate, and filling time based on reinforcement permeability and resin viscosity.
  • Improve mold design: Position injection gates and vents appropriately, and inspect mold sealing, edge gaps, and preform positioning.